GOLDEN RESIN

CH540

Chelating Resins

Home › Product Center › Chelating Resins › CH540
CH540

CH540

CH540 is a macroporous polystyrene resin loaded with nano iron oxide particles. Main application: arsenic removal (effluent arsenic < 8 ppb). Key advantages: nano iron-oxide loading, good bead strength, low pressure drop, and no backwashing required under typical operation.

Inquire Now Tel: +86 15612044421

Product Introduction

CH540 is a macroporous polystyrene resin loaded with nano iron oxide particles. Main application: arsenic removal (effluent arsenic < 8 ppb). Key advantages: nano iron-oxide loading, good bead strength, low pressure drop, and no backwashing required under typical operation.

Typical Physical & Chemical Properties

Polymer matrixPolystyrene crosslinked with divinylbenzene
AppearanceBrown spherical granules
Particle size distribution300 - 1200 µm
< 300 µm (max)1 %
Uniformity coefficient (max)1.7
Packaging density (approx.)790 - 820 g/L (49.4 - 51.2 lb/ft³)
Operating temperature range80 °C (176.0 °F)
pH range (in operation)4.5 - 8.5

Handling, Storage & Loading Notes

  1. Transport & storage. Store the resin in its wet state, preferably above 0 °C. For long idle periods, keep the container closed or add brine of ≥5% NaCl. Protect from freezing during transport, and do not stack heavy objects on top of the resin to avoid crushing the beads.
  2. Pre-treatment. For general requirements, one alkaline → water → acid → water cycle is sufficient; for strict requirements, perform three cycles and finish with the required ionic form.
  3. Loading. Allow for the swelling on form conversion and leave enough freeboard to prevent overflow while keeping a proper liquid level. Keep the column aspect ratio in a reasonable range to avoid channeling. Load wet or backwash to remove air bubbles from the bed.
  4. Feed quality. Before entering the resin column, the liquid should be coagulated, filtered or sand-filtered to ensure it is free of suspended solids that could clog the resin pores.
  5. Idle columns. Resin left idle in a column for a long time must be washed out and stored clean, or kept submerged in brine; it must never dehydrate. Backwash from time to time to loosen the bed and prevent caking.
Chat with Kevin