CH520
CH520 is a macroporous polystyrene chelating resin with N-methyl-D-glucamine groups, drinking-water grade. Main application: boron removal from drinking water. Key advantage: excellent adsorption kinetics. Suitable system: drinking water treatment.
Inquire Now
Tel: +86 15612044421
Product Introduction
CH520 is a macroporous polystyrene chelating resin with N-methyl-D-glucamine groups, drinking-water grade. Main application: boron removal from drinking water. Key advantage: excellent adsorption kinetics. Suitable system: drinking water treatment.
Typical Physical & Chemical Properties
| Polymer matrix | Macroporous polystyrene crosslinked with divinylbenzene |
|---|---|
| Appearance | Spherical granules |
| Functional group | N-methyl-D-glucamine |
| Ionic form | Free base (FB) form |
| Total exchange capacity (min) | 0.6 eq/L (13.1 Kgr/ft³) (FB form) |
| Water retention | 61–67 % (Cl– form) |
| Particle size distribution | 425 - 630 µm |
| < 425 µm | 5 % |
| Uniformity coefficient (max) | 1.2 |
| Swelling, FB → Cl- (max) | 25 % |
| Specific gravity | 1.1 |
| Packaging density (approx.) | 670 - 730 g/L (41.9 - 45.6 lb/ft³) |
| Operating temperature range | 60 °C (140.0 °F) |
Handling, Storage & Loading Notes
- Transport & storage. Store the resin in its wet state, preferably above 0 °C. For long idle periods, keep the container closed or add brine of ≥5% NaCl. Protect from freezing during transport, and do not stack heavy objects on top of the resin to avoid crushing the beads.
- Pre-treatment. For general requirements, one alkaline → water → acid → water cycle is sufficient; for strict requirements, perform three cycles and finish with the required ionic form.
- Loading. Allow for the swelling on form conversion and leave enough freeboard to prevent overflow while keeping a proper liquid level. Keep the column aspect ratio in a reasonable range to avoid channeling. Load wet or backwash to remove air bubbles from the bed.
- Feed quality. Before entering the resin column, the liquid should be coagulated, filtered or sand-filtered to ensure it is free of suspended solids that could clog the resin pores.
- Idle columns. Resin left idle in a column for a long time must be washed out and stored clean, or kept submerged in brine; it must never dehydrate. Backwash from time to time to loosen the bed and prevent caking.