GOLDEN RESIN

D001FG

Food-Grade Resins

Home › Product Center › Food-Grade Resins › D001FG
D001FG

D001FG

D001FG is a macroporous strong acid cation exchange resin on a polystyrene matrix, bearing sulfonic acid groups (–SO₃H). It features uniform pore size, high mechanical strength and a high H-form ratio, and is mainly used in high-velocity mixed-bed water treatment.

Inquire Now Tel: +86 15612044421

Product Introduction

D001FG is a macroporous strong acid cation exchange resin on a polystyrene matrix, bearing sulfonic acid groups (–SO₃H). It features uniform pore size, high mechanical strength and a high H-form ratio, and is mainly used in high-velocity mixed-bed water treatment.

International Equivalents

Amberlite 200, Lewatit Sp-210

Typical Physical & Chemical Properties

AppearanceLight brown opaque beads
Functional group-SO3H
Shipped formNa+
Total exchange capacity≥4.35mmol/g
Volumetric exchange capacity≥1.8mmol/ml
Moisture content45%~55%
True density (wet)1.25~1.28g/ml
Bulk density (wet)0.77~0.85g/ml
Particle size range0.315~1.25mm
Effective particle size0.40-0.70mm
Uniformity coefficient≤1.6
Osmotic-attrition whole bead rate≥90%
Chromaticity≤25APHA
Max. operating temperature120 °C
Resin bed height1~3m
Service flow rate2~10BV/h
Backwash flow rate4~10BV/h
Regeneration (elution) flow rate1~2BV/h
Regenerant dosage2 BV 3~5% HCl, 2 BV 2~4% NaOH

Handling, Storage & Loading Notes

  1. Transport & storage. Store the resin in its wet state, preferably above 0 °C. For long idle periods, keep the container closed or add brine of ≥5% NaCl. Protect from freezing during transport, and do not stack heavy objects on top of the resin to avoid crushing the beads.
  2. Pre-treatment. For general requirements, one alkaline → water → acid → water cycle is sufficient; for strict requirements, perform three cycles and finish with the required ionic form.
  3. Loading. Allow for the swelling on form conversion and leave enough freeboard to prevent overflow while keeping a proper liquid level. Keep the column aspect ratio in a reasonable range to avoid channeling. Load wet or backwash to remove air bubbles from the bed.
  4. Feed quality. Before entering the resin column, the liquid should be coagulated, filtered or sand-filtered to ensure it is free of suspended solids that could clog the resin pores.
  5. Idle columns. Resin left idle in a column for a long time must be washed out and stored clean, or kept submerged in brine; it must never dehydrate. Backwash from time to time to loosen the bed and prevent caking.
Chat with Kevin